Call Us On
+91 97695 84950
Mail Us @
[email protected]
MOKSH TUBES & FITTINGS LLP proudly, supplies, exports, and stocks a wide range of Nickel A286 products, including Pipes & Tubes, Sheets, Plates, Coils, Bars, Forgings, Fasteners, Pipe Fittings, Flanges, Wire Mesh, Welding Rods, and Custom Components designed for high-performance applications.
Alloy A286, also known as AISI 660 or UNS S66286, is a high-strength, iron-nickel-chromium alloy with additions of molybdenum and titanium. It is designed for applications requiring excellent strength and corrosion resistance at temperatures up to 704 °C (1300 °F). It exhibits outstanding mechanical properties and oxidation resistance, making it a widely used material in aerospace, automotive, marine, and industrial gas turbine components.
Get the complete Nickel Based Superalloys A286 datasheet with chemical composition, mechanical properties, heat treatment details, and applications. Enter your email to receive the PDF instantly.
We respect your privacy. Your email will only be used to send the datasheet.
| Category | Details |
|---|---|
| Grade | A286 / Alloy A286 / AISI 660 / UNS S66286 |
| Type | Precipitation-Hardenable Iron–Nickel–Chromium Alloy |
| Temperature Resistance | Up to 704 °C (1300 °F) |
| Strengthening Mechanism | Precipitation Hardening (Ti, Mo, V) |
| Forms Available | Pipes, Tubes, Plates, Bars, Coils, Fittings, Flanges, Fasteners |
| Conditions | Solution Annealed / Aged |
| Certification | EN 10204 3.1 / 3.2 |
| NACE | MR0175 / ISO 15156 Compliant |
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | 24.0 – 27.0 |
| Chromium (Cr) | 13.5 – 16.0 |
| Iron (Fe) | Balance |
| Titanium (Ti) | 1.90 – 2.35 |
| Molybdenum (Mo) | 1.00 – 1.50 |
| Manganese (Mn) | ≤ 2.00 |
| Silicon (Si) | ≤ 1.00 |
| Carbon (C) | ≤ 0.08 |
| Vanadium (V) | 0.10 – 0.50 |
| Sulfur (S) | ≤ 0.030 |
| Phosphorus (P) | ≤ 0.030 |
| Aluminum (Al) | ≤ 0.35 |
| Boron (B) | 0.003 – 0.010 |
Designed for strength + oxidation resistance + stability at high temperatures.
| Temperature | Tensile Strength (MPa) | Yield Strength (MPa) | Hardness (BHN) |
|---|---|---|---|
| 25 °C (80 °F) | 379 | 207 | 145 |
| 425 °C (800 °F) | ~207 | ~124 | ~100 |
| 540 °C (1000 °F) | ~172 | ~103 | ~90 |
| 650 °C (1200 °F) | ~138 | ~83 | ~85 |
| 705 °C (1300 °F) | ~124 | ~69 | ~80 |
| 760 °C (1400 °F) | ~117 | ~62 | ~75 |
Nickel A286 / AISI 660 is engineered for high-temperature, high-stress environments where other alloys fail. It maintains excellent corrosion resistance, good formability, and superior long-term stability in oxidizing conditions.
This alloy meets several recognized industry standards, including:
Nickel Alloy A286 is widely used in environments where thermal stability and mechanical strength are critical. Key applications include:
Nickel A286, also known as AISI 660 or UNS S66286, is a high-strength iron nickel chromium alloy with additions of molybdenum and titanium. It is designed for applications requiring excellent strength and corrosion resistance at temperatures up to 704 °C (1300 °F). The alloy exhibits superior mechanical properties, oxidation resistance, and thermal stability, making it ideal for aerospace, automotive, marine, power generation, and chemical processing applications.
Moksh Tubes & Fittings LLP manufactures, stocks, and exports a wide range of Nickel A286 products including seamless and welded pipes, tubes, sheets, plates, coils, strips, round bars, flat bars, hex bars, square bars, pipe fittings, flanges, fasteners, wire mesh, welding rods, and custom fabricated components. All products are designed for high-performance applications in extreme environments.
Nickel A286 offers high tensile and creep rupture strength even at elevated temperatures, excellent oxidation and corrosion resistance, and long-term dimensional stability. It is easily fabricated and welded, maintains mechanical integrity over prolonged service periods, and is non magnetic after heat treatment. These features make it suitable for critical, high-temperature, high stress industrial applications.
Nickel A286 is widely used in aerospace for jet engines, turbines, exhaust systems, and fasteners; in power generation for turbines, boilers, and high temperature steam systems; in automotive for turbochargers and engine components; in chemical processing for high-temperature equipment; and in oil & gas, marine, and industrial sectors for heat exchangers, subsea tools, and high pressure fasteners.
Moksh Tubes & Fittings LLP provides certified, high performance Nickel A286 products with comprehensive test reports and compliance with international standards. With decades of expertise in nickel based alloys, in house machining, custom fabrication, ready stock for fast delivery, global export capabilities, and dedicated technical support, the company ensures reliable solutions for critical industrial applications.
Connect with Moksh Tubes & Fittings LLP for precision products built for performance.